155 Years Of Glass Production Celebrated

Sklarny Kavalier, Sazava, is the leading Czech manufacturer of flameproof household, technical and laboratory glass. The company, a product of the long tradition of glass manufactuer in Bohemia, also holds an important position among world manufacturers. Sklarny Kavalier, which recently celebrated its 155th anniversary, survived from among the large numbers of small glassworks opened thanks to the "managing abilities" of glassmaker-entrepreneurs.

Author
O Vlasak
Origin
Sklarny Kavalier Co, Czech Republic
Journal Title
Glass Machinery Plants & Accessories 1/95 101-107