Digital Library Publications
Microstructure Of 96% Alumina Ceramics: Ii, Crystallization Of High-Magnesia Boundary Glasses
C A Powell-Dogan, A H Heuer
Refractories
Microstructural Characterisation And Fracture Toughness Of Cordierite-Zro2 Glass-Ceramics
M A Mccoy, A H Heuer
Glass Ceramics
Foaming In Glass Melts Produced By Sodium Sulfate Decomposition Under Isothermal Conditions
D-S Kim, P Hrma
General
Application Of Pure Oxygen With Batch Preheating To Glass-Melting Furnaces
J Tang, A R Cooper
General
Nonisothermal Dissolution Of A Vertical Wall In A Liquid With Temperature Dependent Properties
P Hrma, Y Kamotani
General