Digital Library Publications
Glass Sintering With Concurrent Crystallisation Part 2. Nonisothermal Sintering Of Jagged Polydispersed Particles
M O Prado Et Al
Special Glass
Isothermal Sintering With Concurrent Crystallisation Of Monodispersed And Polydispersed Glass Particles. Part 1
E D Zanotto & M O Prado
Special Glass
Characteristics Of Pb0-Bi01.5-Ga01.5 Glasses Melted In Sn02 Crucibles
J A Cerri Et Al
Special Glass
The Effect Of The Flexure Testing Procedure On The Fracture Statistics Of Glasses
A R Migliore Jnr & E D Zanotto
General